WASHINGTON, D.C. — The School Bus Information Council (SBIC) issued a warning to school bus operators to examine buses in their fleets manufactured by Carpenter and built at the company’s Mitchell, Ind., plant between 1986 and 1995. According to a statement by the SBIC, if defects are found, the buses should be taken off the road immediately.

A notice was originally sent out on April 14, warning about the potential for cracked or broken welds in the roof structure of Carpenter Type C and D school buses. In the following weeks, however, more information became available, and the SBIC added these warnings to school bus operators:

1. Cracked and broken welds in the roof structure have been found in Carpenter buses in various parts of the country and are not solely confined to Florida, where the problem was first discovered.

2. These defects have also been discovered in Type B Carpenter school buses.

3. All Carpenter school buses built at the Mitchell plant between 1986 and 1995 used the same roof design.

4. Every Carpenter school bus has a six-digit number on the Carpenter body data plate. If that number starts with a 4, then the bus was built in the Richmond, Ind., plant and utilizes full-length body bows. This design does not need to be inspected.

Still, the SBIC recommends that school bus operators conduct an inspection of the roof structures in all Carpenter school bus models manufactured at the Mitchell plant. If the six-digit body number starts with anything other than a 4, then the bus should be part of the inspection.

Ron Despenza, transportation director at Clark County (Nev.) School District, was forced to take 23 buses of the road after inspections revealed the roof defects. “We inspected every Carpenter we have, and the problems were obvious,” said Despenza. “We are using spares and standby equipment to cover everything temporarily, but we had to tap into our emergency fund to order bus replacements.”

In New Mexico, state funding has been authorized for the replacement of 64 Carpenter buses. Said Gilbert Perea, state transportation director, “This of course is a juggling act and will delay other replacements for next school year.”

The problem was revealed in March after a school bus rollover accident caused the roof of a 1991 Carpenter to collapse to the seat line. The accident, which occurred in Florida, spurred state officials to advise operators against using Carpenter Type D buses until further investigation was completed.

According to Despenza, many operators are also choosing to repair the problems instead of replacing the buses altogether. But Perea said it could be risky to attempt repairs. “I don’t believe there is a fix for a poor design, and I don’t want to inherit liability on behalf of the state by authorizing a fix,” he said.

The roof welds in question are located at the junction of the vertical side posts — between the windows — and the horizontal structural member above the windows. For more information and photos of the welds, visit www.schoolbusinfo.org.

 

EPA Administrator Christie Whitman steps down

Christie Todd Whitman has announced her resignation as administrator of the U.S. Environmental Protection Agency (EPA), effective June 27, citing a desire to spend more time with her family in New Jersey. Whitman met with President Bush at the White House on May 21 to tender her resignation.

In her resignation letter, Whitman outlined several accomplishments made during her time with the EPA, including the reduction of pollution from diesel engines, aggressive enforcement of environmental laws and monumental Clean Air Act settlements.

Whitman also cited the EPA’s efforts to replace or retrofit older model school buses. Her letter states that the “landmark Clean School Bus USA initiative means that every public school student in America should be riding low emission school buses by 2010.”

In a brief statement released by the White House, the president called Whitman one of the highest-ranking women in his administration and “a trusted friend and adviser.” He also referred to her as a “dedicated and tireless fighter for new and innovative policies for cleaner air, purer water and better protected land.” Bush added a list of contributions made by Whitman that includes the reduction of diesel emissions.

At press time, no replacement for Whitman had been named.


Post a Comment

Request More Info about this product/service/company

Post a comment





Related Stories

Premium Member

Get bus sales numbers, transportation statistics, bus specifications, industry survey results, bus loading and unloading fatality statistics and more in the School Bus Fleet Research Center. Become a premium member today!
Log in Button Register Button

Newsletter

Get breaking news, industry updates, product announcements and more.